Description: Celcon LW90F5 is an M90 based acetal copolymer formulated with a tetrafluoroethylene filler. It is designed for use in wear applications against plastics, metal, glass or ceramic mating surfaces where silicone lubricants can not be tolerated.Information provided by Celanese Corporation. |