MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Daikin POLYFLON™ PTFE M-18 Polytetrafluoroethylene Molding Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Molded

Material Notes: Daikin- Polyflon™ M-18 is a polytetrafluoroethylene virgin granular fine cut resin. This general purpose molding powder has been specifically designed for use in medium to large rod and billet compression molding applications.

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.152 - 2.167 g/ccASTM D 4894
Bulk Density >= 0.490 g/ccASTM D 4894
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 - 60.0 MPaJIS K6891
Elongation at Break >= 450 %JIS K6891
Compressive Yield Strength 7.80 MPa0.2% offset; ASTM D695
 5.00 MPa
@Strain 1 %
ASTM D695
 28.1 MPa
@Strain 25 %
ASTM D695
Compression Set 8.96 %
@Pressure 13.7 MPa,
Time 90000 sec
ASTM D621
 16 %
@Pressure 6.90 MPa,
Time 720000 sec
ASTM D621
 20.1 %
@Pressure 13.7 MPa,
Time 360000 sec
ASTM D621
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+18 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmASTM D257
Dielectric Constant <= 2.1
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 110 kV/mm
@Thickness 0.100 mm
ASTM D149
Dielectric Loss Index <= 0.00010
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point 327 °C
Maximum Service Temperature, Air 260 °C
Shrinkage 2.6 - 3.6 %ASTM D4894
 
Descriptive Properties
AppearanceWhite Powder
MIT Flex5,000,000 cyclesASTM D2178

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daikin POLYFLON™ PTFE M-12 Polytetrafluoroethylene Molding Powder
3M Dyneon™ TF 1620 PTFE
AGC FL1650 PTFE
3M Dyneon™ TF 5050Z PTFE
Beryllium Copper, UNS C17300, TH04 Temper rod, bar, plate, tubing, <9.5 mm

PDAIJ9877 / 209948

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.