MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Saint-Gobain Tygon® 2275 High Purity Tubing Formulation  (discontinued **)
Categories: Polymer; Thermoplastic

Material Notes: Tygon® 2275: Tygon® High Purity Tubing is ideal for handling sensitive fluids such as pharmaceutical or biological solutions. There is virtually no absorption of key fluid constituents into the tubing material or fluid adsorption onto the tubing walls. As a result, fluid alteration and loss is limited. There is no plasticizer to leach into or contaminate the fluid, yet the tubing remains flexible. Tygon® High Purity Tubing can be sterilized by radiation, ethylene oxide, steam or chemical methods. Frequently, incineration is used to dispose of contaminated materials. While many tubings release hazardous by-products when burned, Tygon® High Purity Tubing only releases carbon dioxide and water when properly incinerated, providing safe disposal. Also available with reinforcement to withstand elevated working pressure.

Features and Benefits:
  • Exceptionally low absorption and adsorption compared to silicone
  • Smooth inner surface inhibits particulate entrapment
  • Environmentally safer to dispose; reduces cost of disposal
  • Highly resistant to aggressive cleaners and sanitizers
  • Plasticizer free
  • Meets USP Class VI and FDA requirements for Food Contact
Typical applications include Sterile Filling and Dispensing Systems, Diagnostic Equipment, Nuclear Equipment, Laboratory Analytical Instrumentation, Infusion Sets for Parenterals and Drugs, Cosmetic Production, Food and Beverage Processing, Cell and Tissue Culture Transport.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.900 g/ccASTM D792-91
Water Absorption <= 0.010 %24 hours at 23°C; ASTM D570-95
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 7215 seconds; ASTM D2240-97
Tensile Strength, Yield 2000 psiASTM D412-97
Elongation at Break 700 %ASTM D412-97
100% Modulus 0.350 ksi
@Strain 100 %
ASTM D412-97
Tear Strength 220 pliInitial Tear Strength; ASTM D1004-93
Compression Set 84 %
@Temperature 70.0 °C
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
Tensile Set 187 %ASTM D412-97
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 587 V/milASTM D149-93
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 125 °F
Brittleness Temperature -108 °FASTM D746-95
 -94.0 °FLow Temperature Flexibility; ASTM D380-87
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
ColorClear

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Chemours Teflon® PTFE Grade K-10 Fluoropolymer Resin
Saint-Gobain Norton® Tygon® High-Purity
Saint-Gobain Norton® Tygon® R-1000 Ultra-Soft Tubing Formulation
Saint-Gobain Norton® Tygon® 2075 Ultra Chemical Resistant Tubing Formulation
Saint-Gobain Tygon® A-60-G Industrial Grade Tubing Formulation

PSTGQZ188 / 68702

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.