MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Versalis SINKRAL C433/M3 ABS, Heat Stabilized  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Extruded

Material Notes: Symbol according to ISO 1043-1: ABS

Grade designation according to ISO 2580-ABS 1,EG,095-08-16-15

Special low gloss grade for extrusion and calendering, with high mattness and medium impact resistance. SINKRAL C433/M3 is recommended for the extrusion/co-extrusion of thermoformable sheets in order to produce internal parts of industrial vehicles (door panels, trim, dashboard components), where a low reflectance surface is desired.

Unfilled. Suitable for Profile Extrusion, Sheet Extrusion, Calendering, Thermoforming. Supplied as pellets.

ISO data. Information provided by Enichem

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Key Words: Poly(Acrylonitrile Butadiene Styrene)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/cc
Water Absorption 1.0 %
Moisture Absorption at Equilibrium 0.20 %Humidity Absorption
Melt Flow 6.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
cm³/10 min
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 28.0 MPa50 mm/min
Elongation at Break >= 50 %Nominal
Elongation at Yield 3.0 %50 mm/min
Tensile Modulus 1.40 GPa1 mm/min
Charpy Impact Unnotched NB
 NB
@Temperature -30.0 °C
Charpy Impact, Notched 1.70 J/cm²
 1.00 J/cm²
@Temperature -30.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
Dielectric Strength 30.0 kV/mm
Comparative Tracking Index 600 V
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature 20.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
Vicat Softening Point 98.0 °C50°C/hr; 50N
Flammability, UL94 HB
@Thickness 1.60 mm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENJ76 / 35947

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.