MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
309 Stainless Steel, soft tempered, wire, 12.7 mm diameter
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T 300 Series Stainless Steel

Material Notes: wire > 3.18 mm diameter gage length is 4 times diameter

Key Words: UNS S30900, ASME SA249, ASME SA312, ASME SA358, ASME SA403, ASME SA409, ASTM A167, ASTM A249, ASTM A312, ASTM A314, ASTM A358, ASTM A403, ASTM A409, ASTM A473, ASTM A511, ASTM A554, ASTM A580, FED QQ-S-763, FED QQ-S-766, MIL SPEC MIL-S-862, SAE J405 (30309), DIN 1.4828, X15CrNiSi2012, UNI X 16 CrNi 23 14, B.S. 309 S 24, PN 86022 (Poland), H20N13S2, austenitic
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 147Converted from Rockwell B hardness.
Hardness, Knoop 164Converted from Rockwell B hardness.
Hardness, Rockwell B 85
Hardness, Vickers 169Converted from Rockwell B hardness.
Tensile Strength, Ultimate 725 MPa
Tensile Strength, Yield 620 MPa
@Strain 0.2 %
Elongation at Break 35 %in 50 mm
Modulus of Elasticity 200 GPa
Poissons Ratio 0.30
Shear Modulus 77.0 GPa
Izod Impact 120 - 165 J
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000780 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.9 µm/m-°C
@Temperature 0.000 - 100 °C
 16.7 µm/m-°C
@Temperature 0.000 - 315 °C
 17.3 µm/m-°C
@Temperature 0.000 - 540 °C
 18.0 µm/m-°C
@Temperature 0.000 - 650 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 0.000 - 100 °C
Thermal Conductivity 15.6 W/m-K
@Temperature 0.000 - 100 °C
Melting Point 1400 - 1455 °C
Solidus 1400 °C
Liquidus 1455 °C
Maximum Service Temperature, Air 980 °CIntermittent
 1095 °CContinuous Service
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.20 %
Chromium, Cr 23 %
Iron, Fe 60 %
Manganese, Mn <= 2.0 %
Nickel, Ni 14 %
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
309 Stainless Steel, soft tempered, wire, 1.57 mm diameter
309 Stainless Steel, annealed, bar
309 Stainless Steel, annealed, sheet
309 Stainless Steel, annealed, plate
309 Stainless Steel, annealed, strip

MQ309F / 12713

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.