MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Huber MoldX® S45 Aluminum Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: MoldX® S45 optimized alumina trihydrate is a non-halogen fire retardant product designed for fiberglass reinforced polyester applications such as sheet molding compounds (SMC), bulk molding compounds (BMC) and laminating. MoldX S45 is engineered to allow higher loadings versus standard ATH products and offers excellent processing. The increased loading capability of MoldX S45, from 180 phr to as high as 240 phr in an SMC formulation, eliminates the need for halogen fire retardant additives. SMC compositions containing MoldX S45 as the sole flame retardant can be formulated to meet UL94 VO and UL94 5VA at thicknesses of less than 0.100 inch.

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.42 g/cc
Bulk Density 0.650 g/ccloose
 0.800 g/ccpacked
Brightness 89 %TAPPI
Moisture Absorption 0.300 %
@Temperature 105 °C
Free
Particle Size 9.0 µmMedian Particle Diameter
Particle Mesh Size 325 Mesh0.1% on
 325 Mesh99.9% through
Specific Surface Area 2.0 m²/gBET
 
Component Elements PropertiesOriginal ValueComments
Fe2O3 0.0070 %
Loss on Ignition(%) 34.6 %
@Temperature 1000 °C
Na2O 0.030 %soluble
 0.20 %total
SiO2 0.0050 %
 
Descriptive Properties
Al(OH)3 (%)99.6
FunctionalityRapid Dispersion
 Smoke Suppression
Market/Application: Building & ConstructionCured-In-Place-Pipe
Market/Application: ThermoplasticsPultrusion
Market/Application: ThermosetsWet Mat

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EHUBER756 / 300862

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.