Ti-3Al-2.5V has proved to be a sufficiently malleable material for tube manufacture. It can be cold worked by standard tube making processes, is weldable and can be strength-ended by cold working and subsequent heat treatment to a wide range of strengths and ductilities. Information provided by ATI Wah Chang |