Recycled grade in which carefully reclaimed old parts and production rejects and/or scrap from all processes of manufacturing or processing undergo material recycling. Slightly decreased impact strength compared to BAYBLEND T 64/T 65/T 65MN. Information provided by Bayer. As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
PC + ABS; Poly(Acrylonitrile-Butadiene-Styrene) |