MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dover Chemical MAYSYN S168 Fully Formulated Synthetic Fluid Heavy Duty Machining
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Maysyn S-168 is a high performance, oil rejecting synthetic fluid formulated for the most severe ferrous, as well as nonferrous, applications. Maysyn S-168 is designed to outperform EP-fortified soluble oils and semi-synthetics in most operations. Maysyn S-168 contains no chlorinated, sulfurized, or phosphorus containing additives. In fact, the product’s chemical composition, which provides its complete tramp oil rejection property, makes Maysyn S-168 incompatible with such materials. Maysyn S-168 possesses both low-foaming characteristics, even in dead soft water, and excellent hard water (600 ppm as CaCO3) stability. This makes it suitable for use across a broad spectrum of applications and water conditions, even Blanchard and/or Double Disc Grinding in all areas of soft water. Maysyn S-168, due to its excellent sump life, quick tramp oil rejection, and fine settling characteristics, make it an ideal coolant in either single sump machines or especially central system applications. Longevity is a key item with this product. This product is to be kept from freezing.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/cc
@Temperature 15.6 °C
60/60°F
Density 9.40 lb/gal
pH 8.35% concentration
 8.7Neat
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 50
 
Descriptive Properties
AppearanceClear Yellow
Total Alkalinity8.2[mgHCL/g]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Hydroxypropyl Acrylate
Dow 6D20 Polypropylene Random Copolymer Resin
Dow 221.00 Developmental Performance Polypropylene Polymer

WDOVER142 / 217761

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.