System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Gold 99.99%, Be Modified
Categories:
Metal
;
Nonferrous Metal
;
Precious Metal
;
Gold Alloy
;
Pure Element
Material Notes:
All values may vary dependent on specific design and usage
Beryllium content: 3-7 ppm
Capabilities:
Wire
Ribbon
Square
Insulated
Plated
Information provided by California Fine Wire.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.697
lb/in³
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
18000
psi
Annealed
25000
psi
Stress relieved
32000
psi
Hard
Electrical Properties
Original Value
Comments
Electrical Resistivity
14.14
ohm-cir-mil/ft
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Thermal Properties
Original Value
Comments
CTE, linear
14.2
µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity
0.132
J/g-°C
@Temperature 20.0 °C
Thermal Conductivity
297
W/m-K
Melting Point
1945
°F
Maximum Service Temperature, Air
480
°C
Operating Temperature
Component Elements Properties
Original Value
Comments
Beryllium, Be
0.00030 - 0.00070 %
Gold, Au
99.99 %
Descriptive Properties
Magnetic
None
Temperature Coefficient of Resistance
0.0034 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper
+0.0002 mV
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H00 Temper flat products
Gold, Au
Corundum, Aluminum Oxide, Alumina, 99.9%, Al
2
O
3
Aluminum 6061-T913
Aluminum 6061-T91
MPAuP4 / 12546
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.