MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Henkel Loctite® ABLESTIK ATB 120U Rubberized Epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Appearance: Transparent

Cure: Heat cure

Product Benefits:

  • Non-conductive
  • Fast cure
  • Thin bondline
  • Excellent gap filling ability
  • L2/260ºC performance
Application: Die attach

Filler Type: Silica

Typical Package Application: Die to die stack

Carrier Type: Polyolefin

LOCTITE ABLESTIK ATB 120U adhesive film is formulated for use in wafer lamination processes. It combines process ease with the proven reliability.

Information provided by Loctite®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Moisture Absorption 1.50 %
@Temperature 85.0 °C
Saturation, after 85% RH exposure
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 1.00 MPa
@Temperature 200 °C
Cured, DMTA
 2.00 MPa
@Temperature 250 °C
Cured, DMTA
 3.00 MPa
@Temperature 150 °C
Cured, DMTA
 40.0 MPa
@Temperature 100 °C
Cured, DMTA
 875 MPa
@Temperature 25.0 °C
Cured, DMTA
 2330 MPa
@Temperature -65.0 °C
Cured, DMTA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 62.0 µm/m-°CCured, Below Tg
 238 µm/m-°CCured, Above Tg
Thermal Conductivity 0.210 W/m-KCured
Glass Transition Temp, Tg 75.0 °CCured, TMA
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 minramp to 120°C + 30 minutes @ 120°C
 30.0 minramp to 90°C + 30 minutes @ 90°C + 30 minute ramp to 120°C + 30 minutes @ 120°C
Shelf Life 1.00 MonthUncured, Work life
 9.00 Month
@Temperature 5.00 °C
Uncured, from date of manufacture
 
Descriptive Properties
Extractable Ionic Content (ppm)<10Cured, Chloride (Cl-)
 <10Cured, Fluoride (F-)
 <10Cured, Sodium (Na+)
 <10Cured, Potassium (K+)
Shear Strength2 kg-fDie, 2.5 X 2.5 mm Si die frontside @260°C
 40 kg-fDie, 2.5 X 2.5 mm Si die frontside @25°C
Weight Loss<1%Cured, 300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLOCT5048 / 255259

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.