MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Idemitsu Kosan TARFLON ™ SK2706 Polycarbonate Alloy
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Flame retardant PC alloy grade. High flow, Standard.

Polycarbonate is known for its high impact resistance, good transparency and heat resistance, and superb precision and electrical properties. TARFLON is used in a wide range of applications such as house wares, office equipment , mobile devices, communications equipment, display devices such as LCD backlight parts, automotive, lighting and many fields.

Information provided by Idemitsu Losan Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccISO 1183(JIS K7112)
Moisture Absorption 0.100 %
@Time 86400 sec
50% RH; ISO 62(JIS K7209)
Linear Mold Shrinkage, Flow 0.0040 cm/cm
@Thickness 2.00 mm
Idemitsu Method
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
@Thickness 2.00 mm
Idemitsu Method
Melt Flow 24.2 g/10 min
@Load 2.16 kg,
Temperature 260 °C
ISO 1133 (JIS K7210)
Spiral Flow 40.0 cm
@Thickness 2.00 mm
Width:10mm. Cylinder: 240°C/Mold: 40°C. Inj.Pressure: 125 MPa.; Idemitsu Method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 64.0 MPaISO 527-1,2 (JIS K7161, 7162)
Elongation at Break 50 %Nominal; ISO 527-1,2 (JIS K7161, 7162)
Flexural Strength 90.0 MPaISO 178 (JIS K7171)
Flexural Modulus 3.00 GPaISO 178 (JIS K7171)
Charpy Impact, Notched 10.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1(JIS K7111)
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 36.3 kV/mmIEC 60243-1 (JIS C2110)
 
Thermal PropertiesOriginal ValueComments
CTE, linear 58.0 µm/m-°CISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °CISO 75-1,2 (JIS K7191-1,2)
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °CISO 75-1,2 (JIS K7191-1,2)
UL RTI, Electrical 60.0 °CUL746B
UL RTI, Mechanical with Impact 60.0 °CUL746B
UL RTI, Mechanical without Impact 60.0 °CUL746B
Flammability, UL94 V-1
@Thickness 0.580 mm
 V-0
@Thickness 1.00 mm
 5VB
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 270 °CCylinder Temperature
 <= 280 °CMax Cylinder Temperature
Mold Temperature 40.0 - 70.0 °C
Drying Temperature 80.0 °C
@Time 18000 - 28800 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PIDEM230 / 249594

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.