MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials PEARLBOND® 108 Linear Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: PEARLBOND® 108 is a linear, aromatic polycaprolactone-based polyurethane, supplied in form of white slightly yellowish pellets, which combines a high crystallization rate with a medium thermoplasticity level.

Applications: PEARLBOND® 108 is mainly used for making heat-sealable fabrics (Thermobonding), obtained by coating processes such as scattering or dot-coating (powder or paste). In all cases, the product is previously ground into powder, by cryogenic grinding. The particle size of the powder will depend on the application technique to be used.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccDIN 53.479
Viscosity 3.82e+6 cP
@Temperature 160 °C
Melt viscosity @ 2.16 kg; DIN 53.735
Brookfield Viscosity 350 - 650 cPRVT (15% in MEK); MQSA 55 A
Melt Flow 40 - 90 g/10 min
@Load 2.16 kg,
Temperature 170 °C
DIN 53.735
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 93DIN 53.505
 
Thermal PropertiesOriginal ValueComments
Melting Point 73.0 - 77.0 °CMQSA 70 A
Softening Point 59.0 - 63.0 °CMQSA 70 A
 
Descriptive Properties
Crystallization rate (minutes)HighMQSA 12 B
ThermoplasticityMediumMQSA 68 A

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMES07 / 52905

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.