MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilon® BM-30 FR PA6-MD30 FR
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Mineral Filled

Material Notes:

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.37 g/ccDry; ISO 1183
Water Absorption 8.0 %Sim. to ISO 62
Moisture Absorption 3.00 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0080 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 34.0 MPaConditioned; ISO 527-1/-2
 85.0 MPaDry; ISO 527-1/-2
Tensile Strength, Yield 40.0 MPaConditioned; ISO 527-1/-2
 85.0 MPaDry; ISO 527-1/-2
Elongation at Break 2.5 %Nominal, Dry; ISO 527-1/-2
 45 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 3.0 %Dry; ISO 527-1/-2
 6.0 %Conditioned; ISO 527-1/-2
Tensile Modulus 2800 MPaConditioned; ISO 527-1/-2
 6400 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched 35.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eU
 35.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 40.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eU
 85.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 2.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 3.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 4.00 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°CISO 11359-1/-2
Melting Point 222 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °CLong Term; ISO 2578
 160 °CShort Term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 100 °CISO 75-1/-2
Deflection Temperature at 8.0 MPa 50.0 °CISO 75-1/-2
Flammability, UL94 V-2IEC 60695-11-10
 
Descriptive Properties
Electricals & ElectronicsConnectors
 Electrical equipment
 Energy distribution
FormGranules
ProcessingInjection Molding
Special CharacteristicsFlame retardant
 Improved UV resistance (outdoor use)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Minlon® 73M30 NC010 PA6-MD30
EMS-Grivory Grilon® BM-30 PA6-MD30

PGRH205 / 156914

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.