MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Teknor Apex Monprene® RG-53262 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Monprene RG-53262 is a high performance thermoplastic elastomer, available in NAT and colors, designed for regulated applications including food contact. Monprene RG-53262 is a medium hardness, low density grade with excellent adhesion to PE and complies with various US FDA and European directives for food contact. This grade is suitable for injection molding and extrusion.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Food Contact Acceptable; Good Adhesion; Good Colorability; Good Melt Strength; Good Organoleptic Properties; Good Processability; Halogen Free; High Elongation; Low Density; Medium Hardness; Slip

Uses: Closures; Consumer Applications; Cookware Handles; Cups; Film; Fluid Handling; Food Containers; Food Packaging; Food Service Applications; Gaskets; Kitchenware; Lids; Non-specific Food Applications

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Extrusion; Injection Molding; Press Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 g/ccASTM D792
Melt Flow 9.0 g/10 min
@Load 2.16 kg,
Temperature 175 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 62
@Time 5.00 sec
Injection Molded; ASTM D2240
 64
@Time 1.00 sec
Injection Molded; ASTM D2240
Tensile Strength at Break 550 psiDie C, 20 in/min; ASTM D412
Elongation at Break 500 %Die C, 20 in/min; ASTM D412
 
Processing PropertiesOriginal ValueComments
Processing Temperature 370 - 410 °FMelt, Injection
Rear Barrel Temperature 340 - 380 °FInjection
Middle Barrel Temperature 350 - 390 °FInjection
Front Barrel Temperature 360 - 400 °FInjection
Nozzle Temperature 370 - 410 °FInjection
Zone 1 330 - 370 °FExtrusion
Zone 2 340 - 380 °FExtrusion
Zone 3 350 - 390 °FExtrusion
Zone 4 360 - 400 °FExtrusion
Zone 5 370 - 400 °FExtrusion
Die Temperature 370 - 410 °FExtrusion
Mold Temperature 77.0 - 150 °FInjection
Injection Pressure 200 - 1000 psiInjection
Back Pressure 25.0 - 50.0 psiInjection
Cushion 0.150 - 1.00 inInjection
Screw Speed 30 - 100 rpmExtrusion
 50 - 100 rpmInjection
 
Descriptive Properties
AppearanceColors Available
 Natural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTEKNQ0949 / 237440

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.