MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Toyobo VYLOPET® EMC310TU Injection Molding Polyester Resin, Warpageless, High cycles
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Applications:
  • Coiled bobbins
  • Mouthpieces
Features:
  • High cycles
  • Warpageless

Information provided by Toyobo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.59 g/ccASTM D792
Water Absorption 0.060 %ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cmMD
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 90ASTM D785
Tensile Strength at Break 100 MPaASTM D638
Elongation at Break 2.2 %ASTM D638
Flexural Strength 155 MPaASTM D790
Flexural Modulus 8.80 GPaASTM D790
Izod Impact, Notched 59.0 J/mASTM D256
Taber Abrasion, mg/1000 Cycles 35CS-17; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Dielectric Strength 25.0 kV/mm
@Thickness 2.00 mm
ASTM D149
Arc Resistance 130 secTungsten electrode; ASTM D495
Comparative Tracking Index 250 - 399 VIEC Pub1.112, class 2; IEC Method
 
Thermal PropertiesOriginal ValueComments
CTE, linear 40.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Melting Point 255 °CBy DSC
Maximum Service Temperature, Air 120 °CThermal index; ASTM UL746B
 225 °CBall pressure temperature; IEC Method
Deflection Temperature at 0.46 MPa (66 psi) 240 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 215 °CASTM D648
Flammability, UL94 V-0
@Thickness 0.907 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 255 - 265 °C
Mold Temperature 90.0 - 120 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Toyobo VYLOPET® EMC133 Injection Molding Polyester Resin, Hydrolysis Resistant
Toyobo VYLOPET® EMC132-02 Injection Molding Polyester Resin, Flame Resistant
Toyobo VYLOPET® EMC132-01 Injection Molding Polyester Resin, Flame Resistant
Toyobo VYLOPET® EMC130-20 Injection Molding Polyester Resin, Flame Resistant
Toyobo Vylopet® EMC130-04 Glass Reinforced Polyester, Easy Molding Grade

PTOY650 / 70810

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.