A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is specially formulated to bond to sulfur or peroxide-cured thermoset EPDM rubber for corner molding, end caps and special fixation applications. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for injection molding. It is polyolefin based and completely recyclable. Key Features: - Designed for applications requiring excellent adhesion to vulcanized EPDM rubber.
- Specially formulated to replace thermoset EPDM rubber in automotive glass run channel corner molding applications.
- Designed for shorter processing time compared to thermoset EPDM rubber.
- EU and China RoHS compliant.
Applications:- Automotive- Seals and Gaskets
Uses:- Automotive Applications
- Automotive Exterior Trim
- Bonding
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical |
EU 2003/11/EC; RoHS Compliant |