MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lanxess Uniplex 809 Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Uniplex 809 is a PEG di-2-ethylhexanoate. Uniplex 809 is a high molecular weight liquid plasticizer, having wide compatibility with a variety of polymers. Its low volatility and heat resistance makes it especially useful in engineering plastics, such as polyester and polyamide resins.

Chemical composition: Polyethylene glycol di-2-ethylhexanoate

General Uniplex 809 is characterized by

  • a high molecular weight and its consequent low volatility.
  • a heat resistance making it especially useful in engineering plastics.
  • a good compatibility with a large number of polymers having a certain polarity such as polyesters, polyamides, polyacrylates, polyvinyl acetate and rubbers.
Applications: Uniplex 809 is a high molecular weight liquid plasticizer developed for use in engineering plastics, such as polyester, polyacrylate and polyamide resins. Typical application PET: Used at levels of 4 - 10% on the weight of the PET resin, Uniplex 809 greatly reduces molding respectively processing times. Uniplex 809 offers the advantages of:
  • lowering processing cost
  • enhancing impact resistance
  • low vaporization
  • improving mold releases
  • easily added to the PET resin in single or double screw extruders.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/cc
Viscosity 50 cP
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 1.0[mg KOH/g]
 
Thermal PropertiesOriginal ValueComments
Melting Point -25.0 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4529
Gardner Color Number <= 2.0
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %Karl Fischer
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceClear liquid
Hydroxyl value<2.5 mg KOH/g
Specifications<3 mg KOH/gSum Hydroxyl and Acid Numbers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLANY9112 / 209503

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.