MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ChenGuang CG-A401C Fluoroelastomer Precompounds
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: Description: curatives incorporated fluoroelastomer copolymers or terpolymers

Appearance: off-white, non-transparent slabs

Main grades and Applications: Excellent mold release, good scorch safety.

Recommended for sealing applications that require improved solvent resistance and permeation resistance to fuels, also for fuel tube extrusion

Recommended Vulcanization Formulation for test: Precompounds: 100 phr; MT Carbon Black (N 990): 30 phr; Ca(OH)2: 6 phr; MgO: 3 phr

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.82 g/ccGumstock properties
Viscosity 42 cP
@Temperature 121 °C
ML(1+10), Gumstock properties
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 77Vulcanizate; press cure: 6 min. @177°C; post cure: 24hr. @ 230°C
Tensile Strength at Break 14.0 MPaVulcanizate; press cure: 6 min. @177°C; post cure: 24hr. @ 230°C
Elongation at Break 190 %Vulcanizate; press cure: 6 min. @177°C; post cure: 24hr. @ 230°C
Compression Set 15 %
@Temperature 200 °C,
Time 252000 sec
Vulcanizate; press cure: 6 min. @177°C; post cure: 24hr. @ 230°C
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 66 %Gumstock properties
 
Descriptive Properties
Reological Properties0.3ML, N.m, moving die rheometer, 177oC, 6 min
 0'55"Ts2, moving die rheometer, 177oC, 6 min
 1'55"T90, moving die rheometer, 177oC, 6 min
 2.92MH, N.m, moving die rheometer, 177oC, 6 min

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHENGU010 / 255609

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.