MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Kraton® D1124 K (SIS) Radial Triblock Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Description: Kraton D1124 K is a clear, radial triblock copolymer based on styrene and isoprene, with a polystyrene content of 30%. It is supplied from North America in the physical form identified:
Kraton D1124 K- supplied as a porous pellet.

Region: South America, Europe, Asia Pacific, North America, and Japan

Uses: Kraton D1124 K is used as an ingredient in formulating adhesives, sealants and coatings. It may also find use as a modifier of bitumen or thermoplastics and in compound formulations.

Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Footwear; and Bitumen Modification

Note 1) Primary antioxidant is a non-staining, phenolic antioxidant. The antioxidant package also contains a non-TNPP secondary antioxidant at a target level of 0.2%

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccASTM D4025
Volatiles <= 0.70 %KM 04
Viscosity 340 cP25% Toluene Solution at 25°C; BAM 922
Melt Flow 4.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Ash 0.20 - 0.50 %Talc; BAM 908
 
Chemical PropertiesOriginal ValueComments
Diblock Content 30 %
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 54
@Time 10.0 sec
Typical values on polymer compression molded at 300°F; ASTM D2240
Tensile Strength 14.5 MPaTypical properties on film cast from toluene solution; ASTM D412
Elongation at Break 1100 %Typical properties of film cast from toluene solution; ASTM D412
300% Modulus 0.00296 GPa
@Strain 300 %
film cast from toluene solution.; ASTM D412
 
Descriptive Properties
ContentAntioxidant0.08-0.21%, See Note 1), KM 08
 Polystyrene28-32%, KM 03
 Total Extractables<1.2%, KM 05
Styrene/Rubber Ratio30/70

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kraton® D1193 P (SIS) Linear Triblock Copolymer
Kraton® D2122 DO (SBS) Compound
Kraton® D1124 B (SIS) Branched Triblock Copolymer
Kraton® A1536 H (SEBS) Linear Triblock Copolymer
Kraton® D1126 P (SIS) Radial Copolymer

PKRA9859 / 132758

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.