MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ COLORCOMP™ Compound DX98550H Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP COLORCOMP DX98550H compound is based on Polycarbonate (PC) resin. Added features of this grade include: Low Extractable, Healthcare.

Features: Low Extractable,Aesthetics and Appearance,Healthcare,Custom Color,Food Contact Acceptable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 65.0 MPa5 mm/min; ASTM D638
Elongation at Break 120 %5 mm/min; ASTM D638
Tensile Modulus 2410 MPa5 mm/min; ASTM D638
Flexural Strength 86.0 MPaASTM D790
Flexural Modulus 2340 MPa1.3 mm/min, 50 mm span; ASTM D790
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cmASTM D257
Surface Resistance 1.00e+16 ohmASTM D257
Dissipation Factor 0.010
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 0.00 - 60 secASTM D495
Comparative Tracking Index 100 - 175 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=1.50 mm
UL 746A
 30 - 60 sec
@Thickness >=3.00 mm
UL 746A
 60 - 120 sec
@Thickness >=6.00 mm
UL 746A
High Amp Arc Ignition, HAI 15 - 30 arcs
@Thickness >=1.50 mm
UL 746A
 30 - 60 arcs
@Thickness >=6.00 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 33.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 33.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
UL RTI, Electrical 125 °CUL 746B
UL RTI, Mechanical with Impact 115 °CUL 746B
UL RTI, Mechanical without Impact 125 °CUL 746B
Flammability, UL94 HB
@Thickness >=2.50 mm
UL 94
 V-2
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 305 - 315 °C
Zone 3 310 - 320 °C
Melt Temperature 300 - 315 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80547 / 288494

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.