MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Karina 790-38/23-CRPC Straw CPVC Compound
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: CPVC compound recommended for injection of fitting for use with hot water.

Information provided by Karina Indústria e Comércio de Plásticos Ltda.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 - 1.46 g/ccNBR NM-IEC 60811-1-1
ASTM Color -1.37 - 0.23Color A, ME 12
 14.78 - 16.38Color B, ME 12
 89.54 - 91.14Color L, ME 12
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 77 - 81
@Time 15.0 sec
ASTM D 2240
Tensile Strength >= 400 kg(f)/cm²NBR NM-IEC 60811-1-1
 
Descriptive Properties
ApplicationFittings

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Vycom Corzan® CPVC Chlorinated PVC
Axiall ProTherm® 4526 CPVC Rigid PVC, Molding
Geon® Performance Solutions CPVC LC500 Polyvinyl Chloride, Chlorinated (CPVC)
Vycom FLAMETEC™ CPVC Chlorinated Polyvinyl Chloride Sheet
GEHR Plastics PVC-C®

PKARIN9438 / 171094

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.