MultiQ is a product line of thermoplastic composites in panel form whose specific properties make them particularly suitable as an environmental alternative to plywood in outdoor applications. However, coated with special laminate surfaces, MultiQ can also be used in interiors as an alternative to wood-based panels (HDF and MDF). The MultiQ product line is a modular system. The composition of the glass-reinforced plastic (GRP) sandwich panels offers plenty of scope for variation and permits design to customer specification. MultiQ Impact is a high-performance sandwich panel that has been specially developed as a board for construction scaffolds and other walkways with high levels of demanded impact resistance. The plastic scaffold boards factory-finished with an anti-slip surface are light, extremely impact- and fracture-resistant, non-weathering, non-rotting, easy to clean and extra-durable. |