Multi-purpose with high temperature resistance and strong one-surface bonds. Spray width 1"-3" variable. Bonding range surfaces: one side 10 minunutes, both sides 1 hours. Peel strength is 25 PIW; ITSD T.M. C-449. Coverage is 100 square feet per 24 ounce container. Information provided by 3M Adhesives Division. |