MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Taiwan PU APU-7-800I PU Binder
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Key features:
  • MDI base binder
  • Solvent free
  • One component
  • Good bonding performance
  • Suitable for rubber binding
Description: APU-7-800E, APU-7-800H and APU-7-800I are one-component, moisture-curing and unpigmented PU binders. They can be used for bonding a wide range of substrates, including timber, polystyrene foam, plastic, urethane foam, EPDM granules, recycled rubber, gravel, fabric, aluminum surfaces, etc The curing rate of PU binder is related to the prevailing relative humidity and temperature of the substrates and atmosphere. Curing time can be reduced significantly by use of a hot press on PU binder.

Information provided by Taiwan PU Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 - 1.15 g/cc
Solids Content <= 99 %
Viscosity 3300 - 4300 cP
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 200 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 3.00 - 4.00 hourTack free time
 5.00 - 15.0 minDemold time at110?
 
Descriptive Properties
AppearanceLight yellow viscous liquid
Composition10.8-11.2%NCO

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTAIWPU159 / 305889

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.