MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sandvik 2RK65 Seamless tube and pipe
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Sandvik 2RK65 is an austenitic stainless ELC steel intended for use under severe corrosion conditions within the process industry. The material is characterized by the following properties:
  • very good resistance to attacks in acidic environments, e.g. sulphuric, phosphoric and acetic acid
  • very good resistance to pitting in neutral chloride-bearing solutions
  • much better resistance to crevice corrosion than steels of the AISI 304 and AISI 316 type
  • very good resistance to stress corrosion cracking
  • good weldability
  • Information provided by Sandvik

    UNS N08904; EN 1.4539

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Density 8.00 g/cc
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Vickers 160
    Tensile Strength, Ultimate 520 - 720 MPa
    Tensile Strength, Yield >= 230 MPa
    @Strain 0.2 %
     >= 250 MPa
    @Strain 1 %
     >= 125 MPa
    @Strain 0.2 %,
    Temperature 400 °C
     >= 125 MPa
    @Strain 0.2 %,
    Temperature 400 °C
     >= 136 MPa
    @Strain 1 %,
    Temperature 300 °C
     >= 155 MPa
    @Strain 0.2 %,
    Temperature 200 °C
     >= 155 MPa
    @Strain 1 %,
    Temperature 400 °C
     >= 155 MPa
    @Strain 1 %,
    Temperature 400 °C
     >= 155 MPa
    @Strain 0.2 %,
    Temperature 200 °C
     >= 165 MPa
    @Strain 1 %,
    Temperature 300 °C
     >= 176 MPa
    @Strain 0.2 %,
    Temperature 100 °C
     >= 185 MPa
    @Strain 1 %,
    Temperature 200 °C
     >= 185 MPa
    @Strain 1 %,
    Temperature 200 °C
     >= 205 MPa
    @Strain 0.2 %,
    Temperature 100 °C
    Elongation at Break >= 35 %
     >= 35 %
    @Thickness 50.8 mm
    Modulus of Elasticity 195 GPa
     158 GPa
    @Temperature 500 °C
     166 GPa
    @Temperature 400 °C
     174 GPa
    @Temperature 300 °C
     182 GPa
    @Temperature 200 °C
     190 GPa
    @Temperature 100 °C
     
    Electrical PropertiesOriginal ValueComments
    Electrical Resistivity 0.0000940 ohm-cm
    @Temperature 20.0 °C
     0.0000990 ohm-cm
    @Temperature 100 °C
     0.000107 ohm-cm
    @Temperature 200 °C
     0.000113 ohm-cm
    @Temperature 300 °C
     0.000114 ohm-cm
    @Temperature 500 °C
     0.000115 ohm-cm
    @Temperature 600 °C
     0.000115 ohm-cm
    @Temperature 400 °C
     0.000118 ohm-cm
    @Temperature 700 °C
     
    Thermal PropertiesOriginal ValueComments
    CTE, linear 15.5 µm/m-°C
    @Temperature 30.0 - 100 °C
     16.0 µm/m-°C
    @Temperature 30.0 - 200 °C
     16.0 µm/m-°C
    @Temperature 30.0 - 200 °C
     16.5 µm/m-°C
    @Temperature 300 °C
     17.0 µm/m-°C
    @Temperature 400 °C
     17.0 µm/m-°C
    @Temperature 30.0 - 500 °C
     17.0 µm/m-°C
    @Temperature 30.0 - 400 °C
     17.5 µm/m-°C
    @Temperature 30.0 - 600 °C
     17.5 µm/m-°C
    @Temperature 600 °C
     17.5 µm/m-°C
    @Temperature 30.0 - 700 °C
    Specific Heat Capacity 0.460 J/g-°C
    @Temperature 20.0 °C
     0.485 J/g-°C
    @Temperature 100 °C
     0.485 J/g-°C
    @Temperature 100 °C
     0.515 J/g-°C
    @Temperature 200 °C
     0.545 J/g-°C
    @Temperature 300 °C
     0.545 J/g-°C
    @Temperature 300 °C
     0.570 J/g-°C
    @Temperature 400 °C
     0.590 J/g-°C
    @Temperature 500 °C
     0.590 J/g-°C
    @Temperature 500 °C
     0.605 J/g-°C
    @Temperature 600 °C
     0.615 J/g-°C
    @Temperature 700 °C
     0.615 J/g-°C
    @Temperature 700 °C
    Thermal Conductivity 12.0 W/m-K
    @Temperature 20.0 °C
     14.0 W/m-K
    @Temperature 100 °C
     14.0 W/m-K
    @Temperature 100 °C
     16.0 W/m-K
    @Temperature 200 °C
     18.0 W/m-K
    @Temperature 300 °C
     18.0 W/m-K
    @Temperature 300 °C
     20.0 W/m-K
    @Temperature 400 °C
     22.0 W/m-K
    @Temperature 500 °C
     22.0 W/m-K
    @Temperature 500 °C
     23.0 W/m-K
    @Temperature 600 °C
     25.0 W/m-K
    @Temperature 700 °C
     25.0 W/m-K
    @Temperature 700 °C
     
    Component Elements PropertiesOriginal ValueComments
    Carbon, C <= 0.020 %
    Chromium, Cr 20 %
    Copper, Cu 1.5 %
    Iron, Fe 46.6 %As Balance
    Manganese, Mn 1.8 %
    Molybdenum, Mo 4.5 %
    Nickel, Ni 25 %
    Phosphorus, P <= 0.025 %
    Silicon, Si 0.50 %
    Sulfur, S <= 0.015 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    ATI Allegheny Ludlum Stainless Steel Type 439/AL 439HP™ (ASTM XM-8; UNS S43035)
    Eagle Brass 304 Austenitic Stainless Steel, Full Hardened
    Eagle Brass 304 Austenitic Stainless Steel, 3/4 Hardened
    Sandvik 2R68/2R68HV Seamless tube and pipe
    304 Stainless Steel (UNS S30400); 1/2 Hard Bar, Plate, Sheet, and Strip

    NSANDV230 / 19124

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.