Product description: Grivory GV-5H EF natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. Grivory GV-5H EF natural is used for injection molding technical parts with good surface quality and short cycle times, exhibiting exceptional characteristics even after moisture absorption:- high stiffness and strength
- dimensional stability, low warpage
- good chemical resistance
- good surface finish
Grivory GV is the economical alternative to die-cast alloys.Information provided by EMS Grivory |