MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
BigRep BVOH Butenediol vinyl alcohol copolymer, Filament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: BigRep's BVOH support material is an ecologically friendly advanced water-soluble filament that eliminates post-processing for 3D printed parts. Created for use with dual-extruder printers, BVOH can be used in tandem with any other material to provide efficient support. It has been optimized for improved melt flow, eliminating concerns of hotend clogging that come with other soluble filaments. Due to BVOH's ability to support heavy prints and the support-removal post-processing it eliminates, it's ideal for printing complex, ready-to-use prototypes and objects with large overhang or otherwise complex geometries. BVOH easily dissolves in water - dissolving faster in higher temperatures - cleanly freeing parts from support structures without manual post-processing.

Highlights:

  • Water-soluble
  • Supports heavy prints
  • Nontoxic
  • Odorless

Information provided by Bigrep

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.14 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 34.0 MPaISO 527
Flexural Modulus 2200 MPaISO 178
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point <= 60.0 °CISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 190 °C
 
Descriptive Properties
Filament Net Weight750g, 2.5 and 4.5kg (8.0 kg on request)
Print Bed Temperature60°C
Printing Speed>30 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBIGR007 / 250857

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.