MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
IBC Advanced Alloys Beralcast® 363 Beryllium-Aluminum Alloy
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Beryllium Alloy

Material Notes: This alloy provides an ideal solution for weight, stiffness and thermal critical applications in aerospace, defense and commercial markets. BeAl-363 is a metal matrix composite which consists of 65% Be (by weight) and 35% Al. BeAl-363 is used primarily for high-strength/high-elastic modulus precision cast structural applications. This alloy is 22% less dense than Al-356 and is 3.5 times as stiff.

Information provided by IBC Advanced Alloys

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.16 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 289.6 MPa
Tensile Strength, Yield 213.7 MPa
Elongation at Break 3.0 %
Tensile Modulus 202 GPa
Compressive Yield Strength 226.1 MPa
Bearing Yield Strength 476.4 MPaPin Type (e/D = 2.0)
Poissons Ratio 0.20
Fatigue Strength 117.2 MPa
@# of Cycles 1.00e+7
Axial (R = -1.0)
Shear Modulus 84.2 GPaCalculated
Shear Strength 247.5 MPaPin Double Shear Strength
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000430 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.2 µm/m-°C
@Temperature 25.0 °C
Specific Heat Capacity 1.25 J/g-°C
Thermal Conductivity 105.5 W/m-K
Melting Point 585 °C
Liquidus 585 °C
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 27.75 - 35.05 %As remainder
Beryllium, Be 61.1 - 68.6 %
Cobalt, Co 0.65 - 1.35 %
Germanium, Ge 0.55 - 0.95 %
Iron, Fe <= 0.20 %
Silicon, Si <= 0.50 %
Silver, Ag 2.65 - 3.35 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
IBC Advanced Alloys Beralcast® 191 Beryllium-Aluminum Alloy
Aluminum 6061-T6; 6061-T651
IBC Advanced Alloys Beralcast® 310 Beryllium-Aluminum Alloy
Silver-Copper Eutectic Alloy (72Ag-28Cu; UNS P07720; AWS BAg-8), 10% Cold Work
Silver-Copper Eutectic Alloy (72Ag-28Cu; UNS P07720; AWS BAg-8), 20% Cold Work

NBE363 / 15358

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.