MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
1201 Alloy forged rolled circle
Categories: Metal; Nonferrous Metal; Aluminum Alloy; Other Wrought Al Alloy

Material Notes: Russian Al Alloy used in aerospace cryogenic fuel tanks. Has low density and exhibits high strength, high elasticity, and high fatigue durability at both elevated (up to150°C) and cryogenic temperatures.

Key Words: Russian Aluminum 1201 Alloy, Al-Li Alloys, Aluminium Alloy; Al1201
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.85 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 415 MPa
 600 MPa
@Temperature -253 °C
Tensile Strength, Yield 290 MPa
 350 MPa
@Temperature -253 °C
Elongation at Break 10 %
 14 %
@Temperature -253 °C
Modulus of Elasticity 72.0 GPa
Shear Strength 247 MPaCalculated
 354 MPa
@Temperature -253 °C
Calculated
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000450 ohm-cmEstimated from similar Aluminum alloys
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.8 µm/m-°C
@Temperature 20.0 °C
Estimated from similar Aluminum alloys
 24.5 µm/m-°C
@Temperature 20.0 °C
Estimated from similar Aluminum alloys
Specific Heat Capacity 0.873 J/g-°CEstimated from similar Aluminum alloys
Thermal Conductivity 151 W/m-KEstimated from similar Aluminum alloys

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Magnesium AZ80A-T6, Forged
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Forged Plate
1460 Alloy, forged rolled circle
Clinton Aluminum Alumold® 1-500 Forged
Magnesium AZ80A-F, Forged

MA91201E / 9730

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.