EMERGE™ PC 8702 advanced resin is an ignition-resistant, 20% glass reinforced, polycarbonate resin. This resin contains no bromide, chloride, or phosphate additives. It is a medium flow PC resin with a mold release system, intended for injection molding applications. Applications: - Information Technology Equipment
- Electrical Parts
- Other structural/internal parts
Information provided by Dow This product line was spun off from Dow Chemical to Styron in 2010. |