Durez 33897 is an epoxy-modified, phenolic resin dissolved in Isopropyl Alcohol and Methyl Ethyl Ketone. Durez 33897 is recommended for use in the manufacturing of clutches and torque converters.Information provided by Sumitomo Bakelite High Performance Plastics (sbhpp) |