MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis BorECO™ BA2000 Polypropylene Block Copolymer for Non-Pressure Pipes
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: BorECO™ BA2000 is a high molecular weight, low melt flow rate polypropylene block copolymer with a good balance of mechanical properties. This grade offers superior stiffness while keeping good impact resistance and shows excellent processability. Applications: BorECO™ BA2000 is recommended for solid wall gravity pipes in the application filed of: underground drainage, sewerage, soil, and waste.

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 38.0 MPa50mm/min; ISO 527-2
Elongation at Yield 6.5 %50mm/min; ISO 527-2
Flexural Modulus 2000 MPa1mm/min; ISO 178
Charpy Impact, Notched 2.00 kJ/m²
@Temperature -20.0 °C
ISO 179/1eA
 29.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature 200 - 220 °Ccylinder
Die Temperature 210 - 220 °C
Melt Temperature 210 - 230 °C
Head Temperature 210 - 230 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis BE50-7032 Polypropylene Homopolymer for Non-Pressure pipes and extruded sheets
PolyMirae Moplen EP440G High stiffness sheet Polypropylene Copolymer
LyondellBasell Moplen HP500D Polypropylene
LyondellBasell Moplen EP5079 Polypropylene, Impact Modified; Molded/Extruded
LyondellBasell Hostalen PP H2493 Polypropylene Copolymer

PBOREA338 / 108598

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.