MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik ACRIFIX™ 1R 0192 Bright UV Reactive Cement
Categories: Fluid; Solvent

Material Notes: Product and Use ACRIFIX™ 1R 0192 Bright – One-component polymerization adhesive. Clear, purplish viscous solution of an acrylic polymer in methyl methacrylate, which polymerizes on exposure to light.

Applications: Preferably for transparent edge and area bonds of clear acrylic (PMMA), i.e. ACRYLITE® FF acrylic sheet, ACRYLITE® GP acrylic sheet and parts made of ACRYLITE® molding compounds with one another, but also for other clear plastics such as ABS, PET, PC, PS and PVC.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/cc
Solids Content 30 - 34 %
Brookfield Viscosity 1600 - 2000 cPII/12
 
Thermal PropertiesOriginal ValueComments
Flash Point <= 4.00 °CClosed cup
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.44D68
 
Processing PropertiesOriginal ValueComments
Pot Life 30.0 minat 200 g adhesive
 
Descriptive Properties
ColorClear, slightly purplish

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm Acrylite Plus® zdf Impact Acrylic Polymer
Röhm Acrylite Plus® zk3HR Impact Acrylic Polymer
Röhm Acrylite Plus® zk4BR Impact Acrylic Polymer
Röhm Acrylite Plus® zk4HR Impact Acrylic Polymer
Röhm Acrylite Plus® zk5BR Impact Acrylic Polymer

PEVONIL503 / 196707

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.