Georgia Gulf 7181 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: - Weatherability
- Impact Strength
- Dimensional Stability
- Flame Retardant
- Chemical Resistance
Information provided by Georgia Gulf Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued. |