MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem LL5405S Blown Film Extrusion Linear Low Density Polyethylene  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Blow Molding Grade; Linear Low Density Polyethylene (LLDPE), Extrusion Grade

Material Notes: Description: LL5405S is a Linear Low Density Polyethylene (LLDPE), copolymer of butene-1, produced by Spherilene process and developed for blown film extrusion. Films obtained with this product show a good processing performance balanced with good mechanical properties as well as processability. Very low gel amount.

Additive: Antiblocking – High; Slip - High

Applications: LLDPE and HDPE blends, films with low thickness for general use, bags for waste, special bags for water and protection of clothes.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.918 g/ccASTM D792
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 1070 %ASTM D882
Film Elongation at Break, TD 1340 %ASTM D882
Elmendorf Tear Strength MD 180 gASTM D1922
Elmendorf Tear Strength TD 400 gASTM D1922
Dart Drop Test 130 gF50; ASTM D1709
Film Tensile Strength at Break, MD 40.0 MPaASTM D882
Film Tensile Strength at Break, TD 30.0 MPaASTM D882
1% Secant Modulus, MD 210 MPaASTM D882
1% Secant Modulus, TD 230 MPaASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 12 %ASTM D1003
Gloss 66 %45°; ASTM D2457
 102 %60°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 210 °CProfile
 
Descriptive Properties
Blocking Load8 gf/100cm2ASTM D3354
COF internal0.172h, ASTM D1894

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBRASK2100 / 199981

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.