System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Edinburg Plastics BTP036 PBT Flame Retardant, Talc Filled
Categories:
Polymer
;
Thermoplastic
;
Polyester, TP
;
Polybutylene Terephthalate (PBT)
;
Polybutylene Terephthalate (PBT), Flame Retardant
Material Notes:
Appearance: FR-Stiffness with good surface Colors
Processing Methods: Injection
Applications: Flame Resistant, Less Shrinkage
Information provided by Edinburg Plastics, Inc.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.49
g/cc
ASTM D792-91
Linear Mold Shrinkage
0.0060
-
0.016
cm/cm
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
7600
psi
ASTM D638
Elongation at Break
2.0 %
ASTM D638
Flexural Yield Strength
12500
psi
ASTM D790
Flexural Modulus
400000
psi
ASTM D790
Izod Impact, Notched
0.700
ft-lb/in
ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
68.0
°C
ASTM D648
Flammability, UL94
V-0
@Thickness 0.800 mm
Processing Properties
Original Value
Comments
Rear Barrel Temperature
232
-
249
°C
Middle Barrel Temperature
243
-
260
°C
Front Barrel Temperature
249
-
266
°C
Nozzle Temperature
243
-
260
°C
Melt Temperature
257
°C
Mold Temperature
49.0
-
82.0
°C
Drying Temperature
121
°C
Dry Time
3.00
-
12.0
hour
Moisture Content
<= 0.20 %
Dew Point
>=
-40.0
°F
Back Pressure
50.0
-
80.0
psi
Lower is better
Screw Speed
40
-
80
rpm
Lower is better
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
Kingfa PBT-T30 30% Mineral Filled PBT
Hanwha Azdel AZMET® CM20350 35% continuous random fiber mat / PBT resin matrix
Evonik Vestodur® RS 1441 30% Mineral Reinforced, Radiation Crosslinkable PBT
Evonik Vestodur® RS 1409 30% Mineral Reinforced, Radiation Crosslinkable PBT
PEDIN044 / 183547
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.