MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SPHERE ONE EXTENDOSPHERES™ SLG Hollow Spheres
Categories: Ceramic; Oxide; Silicon Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: EXTENDOSPHERES™ SL are white, low-cost, low-density ceramic hollow spheres.

Applications: With a density of 0.73 g/cc and a crush strength of 3,000 psi, these hollow spheres are ideal for use in coatings, sealants, caulks and other applications where low shrinkage, lightweight and white particles are desired.

Information provided by Sphere One Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.400 g/cc
Density 0.730 g/cc
Particle Size 120 - 130 µmMean
 10 - 300 µm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Mohs 5.0
Compressive Strength 3000 psi
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1700 °CDeformation temp
 
Component Elements PropertiesOriginal ValueComments
Al2O3 38.5 %
Fe2O3 0.50 %
SiO2 59 %
TiO2 1.7 %
 
Descriptive Properties
ColorOff White
Physical FormFree-Flowing Powder
Shell ThicknessApprox. 10% of diameter

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow SYL-OFF® 7367 CROSSLINKER
Lanxess Vulkasil® A1 Precipitated Silica Filler for Rubber
Imerys NYCOR® R Wollastonite
Imerys M1250 AS WOLLASTOCOAT® Wollastonite
Eastman Saflex® 0.030 inch Clear Protective Interlayer PVB Film for Glass Laminates

CSPHERE07 / 2203

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.