MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Evonik TEGO® Antifoam PS 10 Emulsion
Categories: Other Engineering Material

Material Notes: Product description: TEGO® Antifoam PS 10 is an emulsion based on modified siloxanes.

Application: TEGO® Antifoam PS 10 is useful as defoamer in various textile applications. It is efficient as antifoam in application where surfactants and various surfactant blends/formulations are used e. g. scouring etc. TEGO® Antifoam PS 10 is also used as antifoam in dyeing processes where high shear rates occur (e. g. jet machines).

Properties / Benefits: The special combination of active ingredients provides TEGO® Antifoam PS 10 with excellent stability in alkaline or electrolyte-rich media, even at high temperatures. With regard to compatibility, dispersability and handling, TEGO® Antifoam PS 10 performs much better then conventional silicone antifoams. Furthermore, the undesirable effects associated with silicone based antifoams (e. g. silicone spotting) are either significantly reduced or totally eliminated.

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 - 1.04 g/cc
Solids Content 10 - 12 %
pH 6.0 - 8.0
 
Descriptive Properties
Appearancewhite liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik SIPERNAT® 383 DS Silica Powder
Evonik SIPERNAT® D 17 Silica Powder
Evonik SIPERNAT® D 13 Silica Powder
Evonik SIPERNAT® D 10 Ceramic Powder
Evonik SIPERNAT® 50 Silica Powder

PEVONIL557 / 196761

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.