MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik VESTAKEEP® 1000 G Polyetheretherketone (PEEK)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Low- viscosity, unreinforced polyether ether ketone VESTAKEEP® 1000G is a low-viscosity, unreinforced polyether ether ketone for injection molding. The semi-crystalline polymer features superior, thermal and chemical resistance. Parts made from VESTAKEEP® 1000G are self-extinguishing. VESTAKEEP® 1000G can be processed by common injection machines for thermoplastics. VESTAKEEP® 1000G is supplied as granules in 25 kg boxes with moisture-proof polyethylene liners.

Property data for dry samples.

Information provided by Evonik.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccISO 1183
Water Absorption 0.50 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0090 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cmISO 294-4, 2577
Melt Flow 150 g/10 min
@Load 5.00 kg,
Temperature 380 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 100 MPaISO 527
Elongation at Break 10 %Nominal; ISO 527
Elongation at Yield 5.5 %ISO 527
Tensile Modulus 3900 MPaISO 527
Charpy Impact Unnotched 60.0 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eU
 60.0 kJ/m²
@Temperature -30.0 °C
Complete Break; ISO 179/1eU
Charpy Impact, Notched 5.00 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eA
 5.00 kJ/m²
@Temperature -30.0 °C
Complete Break; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+13 ohm-cmIEC 62631-3-1
Surface Resistance 1.00e+14 ohmIEC 62631-3-2
Dielectric Constant 2.8
@Frequency 1e+6 Hz
IEC 62631-2-1
Dielectric Strength 16.0 kV/mmS20/P50; Sim. to IEC 60243-1
 19.0 kV/mmS20/S20; IEC 60243-1
Comparative Tracking Index 175 Vtest solution A, 100 drops value; IEC 60112
 200 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 340 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 205 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 155 °CISO 75-1/-2
Vicat Softening Point 310 °CMethod B: 10 N, 50 K/h; ISO 306
 335 °CMethod A: 10 N, 50 K/h; ISO 306
Glass Transition Temp, Tg 150 °CISO 11357-1/-2
Flammability Test 5.0
@Thickness 1.60 mm
IEC 60695-11-10
Oxygen Index 38 %ASTM D 2863
Glow Wire Ignition Temperature 800 °CIEC 60695-2-13
Glow Wire Flammability Index 960 °CIEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Melt Temperature 360 - 380 °C
Mold Temperature 160 - 200 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ensinger Tecapeek® Polyetheretherketone (PEEK)
Afton Plastics 450G PEEK Polyetheretherketone
GEHR Plastics PEEK Polyetheretherketone
Ensinger Tecapeek® XP-96 Compression Molded PEEK
Afton Plastics 450FC30 PEEK 30% Carbon Fiber Filled Polyetheretherketone

PEVONIK805 / 243014

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.