JFoam™ HTC-18-R is the B component of a two part polyurethane modified polyisocyanurate system, which when combined with the A component will produce an all water-blown rigid polyurethane / polyisocyanurate foam system. HTC-18 can be used in core foam applications requiring high compressive strengths and modulus at high temperatures.Information provided by J6 Polymers LLC |