MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Go Yen Chemical GOYENCHEM-CT Cyclic Phosphonate Flame Retardant CU 93%
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CAS No.41203-81-0

Intro: GO YEN CHEMICAL INDUSTRIAL CO., LTD. is a major player in chemical industry and now is the largest manufacturer of flame retardants and fine chemicals in Taiwan. We also provide a series of total solutions for our customers. GOYENCHEM-CT ( equivalent RHODIA Amgard CT ) is a cyclic phosphonate and non-halogenated flame retardantthat is developed by GYC GROUP. With great amount of phosphonates, GOYENCHEM-CT provides exceptional and durable flame retardancy to the fabrics especially polyester ones that the flame retardant performance remains excellent after several home laundries. Containing no halogens, formaldehyde, and antimony, the flame retardant has no harm to human bodies. GOYENCHEM-CT features great physical properties and processability that barely causes yellowing for the finished textile and keeps pleasant touch of the fabrics as it is suited for applications in soft furnishings, toys, various fabrics, etc.

Advantages:

  • Non-halogenated flame retardant
  • Contains no formaldehyde and antimony
  • Provides excellent and durable flame retardancy to the fabrics
  • Flame retardant performance remains excellent after several home laundries
  • Excellent physical properties and processability
  • Offers ease of operating
  • Barely causes yellowing for the finished textile
  • Keeps pleasant touch of the fabrics
Applications:
  • Any kinds of fabrics especially polyester ones
  • Soft furnishings: curtains, rugsā€¦
  • Cotton
  • Silk
  • Nylon
  • Toy industry

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 93 %
pH 2.0 - 3.0
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 20
 
Processing PropertiesOriginal ValueComments
Moisture Content 6.8 - 7.0 %
 
Component Elements PropertiesOriginal ValueComments
Phosphorus, P 19 %
 
Descriptive Properties
AppearanceLiquid
Color<100
 Colorless to light yellow
Composition<0.5DMMP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN182 / 266490

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.