Description: - Aramid fiber-based, carbon loaded, flat surface honeycomb absorber.
- Designed to provide good absorption across a wide range of frequencies.
- Ideal for antenna cross-talk and sidelobe reduction, cavity resonance suppression, and far-field electromagnetic applications.
- Can be water-jet or machine cut for custom configurations.
- RoHS and REACH compliant.
Information provided by Hexcel Corporation. |