MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 595°C (1100°F) for 2 hours
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal galling. Applications in the aerospace industry, including parts in military and commercial gas turbine engines.

Data provided by the manufacturer, Haynes International, Inc.

Key Words: UNS R30605, AMS 5537, AMS 5759, AMS 5796, AMS 5795
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 9.13 g/ccat RT
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 1315 MPa
 290 MPa
@Temperature 980 °C
 490 MPa
@Temperature 870 °C
 800 MPa
@Temperature 760 °C
 965 MPa
@Temperature 650 °C
 1025 MPa
@Temperature 540 °C
 1140 MPa
@Temperature 315 °C
Tensile Strength, Yield 1115 MPa
@Strain 0.2 %
 215 MPa
@Strain 0.2 %,
Temperature 980 °C
 345 MPa
@Strain 0.2 %,
Temperature 870 °C
 635 MPa
@Strain 0.2 %,
Temperature 760 °C
 820 MPa
@Strain 0.2 %,
Temperature 650 °C
 855 MPa
@Strain 0.2 %,
Temperature 540 °C
 910 MPa
@Strain 0.2 %,
Temperature 315 °C
Elongation at Break 16 %in 51 mm
 7.0 %
@Temperature 760 °C
in 51 mm
 9.0 %
@Temperature 870 °C
in 51 mm
 12 %
@Temperature 980 °C
in 51 mm
 13 %
@Temperature 650 °C
in 51 mm
 23 %
@Temperature 540 °C
in 51 mm
 28 %
@Temperature 315 °C
in 51 mm
Modulus of Elasticity 225 GPaRT
 146 GPa
@Temperature 1000 °C
 154 GPa
@Temperature 900 °C
 163 GPa
@Temperature 800 °C
 174 GPa
@Temperature 700 °C
 181 GPa
@Temperature 600 °C
 188 GPa
@Temperature 500 °C
 197 GPa
@Temperature 400 °C
 204 GPa
@Temperature 300 °C
 214 GPa
@Temperature 200 °C
 222 GPa
@Temperature 100 °C
Charpy Impact 262 J
 144 J
@Temperature 980 °C
 148 J
@Temperature -196 °C
 163 J
@Temperature 870 °C
 182 J
@Temperature -138 °C
 194 J
@Temperature 760 °C
 212 J
@Temperature -78.0 °C
 230 J
@Temperature 650 °C
 243 J
@Temperature -29.0 °C
 273 J
@Temperature 540 °C
 297 J
@Temperature 260 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000886 ohm-cmRT
 0.0000950 ohm-cm
@Temperature 1000 °C
 0.0001011 ohm-cm
@Temperature 900 °C
 0.0001066 ohm-cm
@Temperature 700 °C
 0.0001078 ohm-cm
@Temperature 800 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.3 µm/m-°C
@Temperature 25.0 - 100 °C
 12.9 µm/m-°C
@Temperature 25.0 - 200 °C
 13.6 µm/m-°C
@Temperature 25.0 - 300 °C
 14.3 µm/m-°C
@Temperature 25.0 - 500 °C
 14.3 µm/m-°C
@Temperature 25.0 - 400 °C
 14.6 µm/m-°C
@Temperature 25.0 - 600 °C
 15.1 µm/m-°C
@Temperature 25.0 - 700 °C
 15.8 µm/m-°C
@Temperature 25.0 - 800 °C
 16.5 µm/m-°C
@Temperature 25.0 - 900 °C
 17.0 µm/m-°C
@Temperature 25.0 - 1000 °C
Thermal Conductivity 9.40 W/m-KRT
 10.9 W/m-K
@Temperature 100 °C
 12.9 W/m-K
@Temperature 200 °C
 14.8 W/m-K
@Temperature 300 °C
 16.8 W/m-K
@Temperature 400 °C
 18.7 W/m-K
@Temperature 500 °C
 20.7 W/m-K
@Temperature 600 °C
 22.6 W/m-K
@Temperature 700 °C
 24.7 W/m-K
@Temperature 800 °C
 26.7 W/m-K
@Temperature 900 °C
 29.2 W/m-K
@Temperature 1000 °C
Melting Point 1330 - 1410 °C
Solidus 1330 °C
Liquidus 1410 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.10 %
Chromium, Cr 20 %
Cobalt, Co 51 %
Iron, Fe <= 3.0 %
Manganese, Mn 1.5 %
Nickel, Ni 10 %
Silicon, Si <= 0.40 %
Tungsten, W 15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Haynes 25 alloy, cold worked sheet, 20% cold reduction
Haynes 25 alloy, room temperature after 25% cold reduction, 1120°C anneal for 5 minutes
Haynes 25 alloy, room temperature after 25% cold reduction, 1065°C anneal for 5 minutes
Haynes 25 alloy, room temperature after 20% cold reduction
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 55% Cold Reduction

NH25BS / 16598

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.