MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LNP™ THERMOCOMP™ Compound LC006EXQ Polyetheretherketone (PEEK)
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: LNP THERMOCOMP LC006EXQ compound is based on Polyetheretherketone (PEEK) resin containing 30% carbon fiber. Added features of this grade include: Electrically Conductive, Easy Molding.

Features: High Stiffness,Light-weight Structural,High Heat Resistance,Super Strong (Carbon Fiber Filled),Electrically Conductive,Easy Molding,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 g/ccASTM D792
Moisture Absorption 0.0500 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0015 - 0.0030 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0070 - 0.014 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 314 MPa5 mm/min; ASTM D638
 319 MPa5 mm/min; ISO 527
Elongation at Break 1.5 %5 mm/min; ISO 527
 1.7 %5 mm/min; ASTM D638
Tensile Modulus 31700 MPa5 mm/min; ASTM D638
 35320 MPa1 mm/min; ISO 527
Flexural Strength 457 MPaISO 178
 477 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 27100 MPa1.3 mm/min, 50 mm span; ASTM D790
 27230 MPa2 mm/min; ISO 178
Poissons Ratio 0.44ASTM E132
Shear Modulus 4.756 GPaASTM D732
Shear Strength 119 MPaASTM D732
Izod Impact Notched 75.0 JASTM D256
Izod Impact, Unnotched 936 J/mASTM D4812
Dart Drop, Total Energy 6.00 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1000 - 10000 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 5.00 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E831
CTE, linear, Transverse to Flow 30.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E831
Deflection Temperature at 1.8 MPa (264 psi) 332 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 380 - 400 °C
Zone 3 380 - 400 °C
Mold Temperature 175 - 190 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa
Screw Speed 60 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81670 / 289617

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.