MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Petropol Makropol® A3 DF5 MF UV BRC0432 PC376 PC, 50% RH
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: Product Description: High Viscosity, UV Stabilized, Polycarbonate. Makropol DF grades have good diffusivity appropriate for LED lighting.

Resin ID (ISO 1043): PC
Additive: Up Resistant; Diffuse
Processing: Extrusion
Color: Haze

Information provided by Petropol

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 0.12 %Equilibrium; ISO 62
Water Absorption at Saturation 0.30 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 75.0 MPaASTM D638
Tensile Strength, Yield 65.0 MPa50 mm/min; ISO 527-1-2
Elongation at Break 75 %50 mm/min; ISO 527-1-2
Elongation at Yield 6.3 %50 mm/min; ISO 527-1-2
Tensile Modulus 2350 MPa1mm/min; ISO 527-1-2
Flexural Strength 96.0 MPa2 mm/min; ISO 178
Flexural Modulus 2350 MPa2 mm/min; ISO 178
Flexural Strain at Break 7.2 %2 mm/min; ISO 178
Izod Impact, Notched (ISO) 16.0 kJ/m²
@Temperature -30.0 °C
ISO 180-A
 90.0 kJ/m²
@Temperature 23.0 °C
ISO 180-A
Charpy Impact Unnotched NB
@Temperature -30.0 °C
ISO 179-1eU
 NB
@Temperature 23.0 °C
ISO 179-1eU
Charpy Impact, Notched 18.0 kJ/m²
@Temperature -30.0 °C
ISO 179-1eA
 80.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohmIEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 100 Hz
IEC 60250
Dielectric Strength 33.0 kV/mm
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor 0.00050
@Frequency 100 Hz
IEC 60250
 0.0085
@Frequency 1e+6 Hz
IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1,-2
Thermal Conductivity 0.200 W/m-KISO 8302
Melting Point 280 °CISO 294
Deflection Temperature at 0.46 MPa (66 psi) 141 °CISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 129 °CISO 75-1,-2
Vicat Softening Point 149 °C
@Load 5.10 kg
50°C/h; ASTM D1525A
 150 °C
@Load 5.10 kg
120°C/h; ASTM D1525A
Flammability, UL94 HB
@Thickness 2.90 mm
 V-2
@Thickness 0.750 mm
 V-2
@Thickness 1.50 mm
 V-2
@Thickness 2.80 mm
Glow Wire Test 850 °C
@Thickness 1.00 mm
IEC 60695-2-12
 850 °C
@Thickness 1.50 mm
IEC 60695-2-12
 850 °C
@Thickness 2.00 mm
IEC 60695-2-12
 850 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 290 °CMolding
Mold Temperature 70.0 - 90.0 °C
Drying Temperature 120 °C
Dry Time 4.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPETROPOL036 / 312944

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.