Product Description: Medium melt flow rate homopolymer designed for high speed extrusion of woven fabrics exhibiting low water carry over. Availability: North America Features: - Balanced Stiffness/Toughness
- General Purpose
- Low Water Carryover
Uses: - Carpet Backing
- Compounding
- Fabrics
- Fibers
- Packaging
Processing Method: ExtrusionInformation provided by ExxonMobil Chemical |