MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
HB Fuller HydroArmor® 7755 Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Description: HydroArmor® 7755 is a sprayable latex coating designed for use on aluminum, fiberglass, cold rolled steel, galvanized steel and most metal primers. HydroArmor® 7755 is formulated to give very good corrosion protection when applied as thin as 20 mils wet. This low viscosity, sag resistant coating can be easily sprayed onto exposed underbody areas, and into restricted areas such as tubing and “hidden” areas accessible only with spray wands; wet film builds of 30 mils or more can be applied without runs, drips or sags. Our lab tests of HydroArmor® show this coating is extremely durable under even the worst service conditions: several days at 121°C (250°F) and immersion in acidic and caustic solutions did not affect the dried film; rocks bounced off the coating when test panels were subjected to the “Gravelometer” at -34°C (-30°F). After 1500 hours in the salt spray cabinet, the HydroArmor coating remains intact and there is no corrosion under the coating. HydroArmor® dries quickly at ambient temperatures and will withstand urethane paint bakes after only 30 minutes dry time at room temperature. Tex house paint. HydroArmor® provides better protection than any of the competitive products we’ve tested without environmental and safety problems inherent in many of the under coatings available today.

Application: As with any coating, all loose dirt and rust should be removed before application. HydroArmor® is designed to be applied with airless spray equipment. We recommend that a minimum of 20 wet mils be applied for optimum performance. We have sprayed this product with a 30:1 airless pump with a Graco airless spray gun. With this equipment, we can spray at 40 to 50 pounds air pressure using spray tips with orifices from .015” to .027”. HydroArmor® resists water wash-off after air drying 30 minutes at 45-55% relative humidity; if not baked, it dries through in 24 hours or less (drying is slowed by high humidity and poor air circulation). Until HydroArmor ® dries, overspray can be removed and equipment can be cleaned with water. Dried material can be removed with Methyl Ethyl Ketone.

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.44 - 1.50 g/cc
Solids Content 69 - 73 %
Volatile Organic Compounds (VOC) Content 10 - 13 g/l
pH 9.0 - 10
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL161 / 316952

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.