MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Hybrid Plastics Polyamide POSS® Flow Masterbatch
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: POSS® Flow masterbatches show success in reducing the melt viscosity of a variety of injection molded and extruded resins. Hybrid Plastics now introduces such a solution for polyamide polymers. Polyamide POSS® Flow is a pellet masterbatch incorporating POSS® that can be used directly in the process or manufacturing stream. For injection molding applications, benefits include decreased molding pressures and increased flow for filling intricate and thin-walled parts. This leads to faster cycle times and less scrap. For extrusion applications, POSS® Flow decreases screw torque, allowing increased extrusion rates.

At loading levels of up to 10%, Polyamide POSS® Flow does not significantly affect mechanical properties such as modulus, yield strength, or elongation to break. At a 20% loading, there is only a minor decrease in modulus and yield strength.

This product is offered in two different versions. Polyamide POSS® Flow is for use in systems without particles or fillers. Polyamide POSS® Flow with POSS® Dispersant combines two POSS technologies into one product. POSS® Flow decreases melt viscosity, while POSS® Dispersant coats and disperses particles reducing melt viscosity even further, thereby increasing productivity and allowing up to three times as much filler to be added.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/cc
Filler Content 10 - 20 %
Melt Flow 110 g/10 min
@Load 2.16 kg,
Temperature 180 °C
 
Thermal PropertiesOriginal ValueComments
Melting Point 170 °C
Decomposition Temperature 350 °C5% wt loss in N2
 
Descriptive Properties
Colortranslucent, light brown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHYBR038 / 88746

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.