Data provided by DuPont Packaging Polymers. An exceptionally strong Mylar® polyester film designed to package foods. Foods can be heated or cooked in this film at temperatures up to 204°C (400°F). Seal side is wound to the core. This film, when laminated to foil, makes an excellent inner cap seal for PET jars. This film is also suitable for heating food products in microwave or conventional ovens. |